Vapour phase decomposition

Vapour phase decomposition (VPD) is a method used in the semiconductor industry to improve the sensitivity of total-reflection X-ray fluorescence spectroscopy by changing the contaminant from a thin layer (which has an angle-dependent fluorescence intensity in the TXRF-domain) to a granular residue. In granular residue the limits of detection are improved because of a more intense fluorescence signal in angles smaller than the isokinetic angle. A related technique is VPD-DC (vapour phase decomposition-droplet collection), the wafer is scanned with a droplet that collects the metal ions that were dissolved in the decomposition step. This procedure affords better limits of detection when applying atomic absorption spectroscopy (AAS) in order to detect metal impurities of very small concentrations on wafer surfaces.

This can be achieved by enhancing the impurity concentration in the solution to be analyzed. In standard AAS, the impurity is dissolved together with the matrix element. In VPD, the surface of the wafer is exposed to hydrofluoric acid vapour, which causes the surface oxide to dissolve together with the impurity metals. The acid droplets, condensed on the surface, are then analyzed using AAS.

The method has yielded good results for the detection and measurement of nickel and iron.

To improve the range of elemental impurities and lower detection limits, the acid droplets obtained from the silicon wafers are analyzed by ICP-MS (Inductively coupled plasma mass spectrometry). This technique, VPD ICP-MS provides accurate measurement of up to 60 elements and detection limits of in the range of 1E6-E10 atoms/sq.cm on the silicon wafer.

This article is issued from Wikipedia - version of the 5/22/2016. The text is available under the Creative Commons Attribution/Share Alike but additional terms may apply for the media files.